Item | Unit | Standard | Typical | Testing device and method thereof | |
---|---|---|---|---|---|
Chemical composition | Ni+Co+Mn | % | 59.00±1.00 | 58.81 | EDTA titration |
Ni | % | 49.00±1.00 | 48.83 | ICP | |
Co | % | 6.80±0.50 | 6.77 | ICP | |
Mn | % | 3.30±0.50 | 3.35 | ICP | |
Impurity | Fe | ppm | ≤100.0 | 34.0 | ICP |
Na | ppm | ≤100.0 | 45.0 | ICP | |
Cu | ppm | <20.0 | 1.0 | ICP | |
ParticleSize distribution | D10 | μm | ≥5.00 | 5.59 | MasterSize3000,Laser Particle Size analyser; Hydro3000MU; Sample amount: 2g; Dispersant: water; Refractive index: 1.330; |
D50 | μm | 10.50±1.00 | 10.80 | ||
D90 | μm | ≤25.00 | 17.90 | ||
D99 | μm | ≤30.00 | 23.30 | ||
pH | / | 11.75±0.20 | 11.76 | pH meter | |
Li impurities | Li₂CO₃ | % | ≤0.3000 | 0.1100 | Acid-base Titration |
LiOH | % | ≤0.4500 | 0.3600 | ||
Moisture | ppm | ≤400 | 257 | Karl Fischer | |
BETSurfaceArea | m²/g | 0.300-0.600 | 0.450 | 3H-2000A; Adsorbent: High purity N2: He=4:1; BET tube: 9mm U-shaped tube |
|
Tap Density | g/cm³ | ≥2.200 | 2.500 | Tap density meter: Vibration frequency: 100~300 times/min; Width: 3mm; Vibration times: 4000 times; Cartridge 100 ml; sample volume 100g; |
|
1sDischarge Capacity | mAh/g | ≥208.0 | 208.7 | CR2032 battery0.1C/0.1C,4.3~3.0V | |
1st efficiency | % | ≥88.00 | 89.40 |
Lithium ion Battery NCM High Nickel Cathode Ni83
This lithium nickel cobalt manganese oxide (NCM) cathode material exhibits high capacity, low initial impedance, excellent cycling stability, and slow impedance growth, making it well-suited for medium- and small-sized lithium-ion batteries.”